MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

ITW Devcon Composite Welder™ Methacrylate Adhesive FS, Blue Green, Black
Categories: Polymer; Adhesive; Thermoset; Methacrylate; Methacrylate Adhesive

Material Notes:

Information provided by ITW Devcon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 120000 cP120000 cPMixed Viscosity (Thixotropic gel)
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break 100 - 125 %100 - 125 %
Adhesive Bond Strength 15.5 MPa2250 psilap shear (on grit blasted steel, bond line thickness of 0.010"); ASTM D1002
Tensile Impact Strength 46.2 kJ/m²22.0 ft-lb/in²
Peel Strength 10.5 - 11.4 kN/m60.0 - 65.0 pli
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °Fdry
Minimum Service Temperature, Air -40.0 °C-40.0 °Fdry
 
Processing PropertiesMetricEnglishComments
Cure Time 10.0 - 15.0 min0.167 - 0.250 hourFixture time
 45.0 - 60.0 min0.750 - 1.00 hourFunctional cure
Working Life 4.00 - 8.00 min4.00 - 8.00 min
 
Descriptive Properties
Mix ratio (Resin:Hardener)10:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Titanium Ti-6Al-4V ELI (Grade 23), Annealed
TIMET TIMETAL® 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Rod or Thickness, <3.00 in, Annealed, Per ASTM B348
TIMET TIMETAL® 6-4 ELI Titanium Alloy (Ti-6Al-4V ELI; ASTM Grade 23) (Annealed; 1.75 - 2.50 in Rod or Thickness; Per ASTM F136)
Permabond TA4810 Toughened Acrylic Adhesive
Overview of materials for Methacrylate Adhesive

PITW15 / 48464

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.