MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Evonik EUROPLEX® Film HC 0F046 PMMA  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Acrylic (PMMA)

Material Notes: Product: EUROPLEX® Film HC 0F046 is a weather resistant, transparent and optical quality co-extruded PMMA and PVDF film for graphic lamination systems. This film displays excellent performance in long term outdoor weathering without experiencing color change or yellowing. EUROPLEX® Film HC 0F046 provides high protection for other polymeric substrates against degradation caused by UV radiation. Due to its PVDF top layer, the film displays very good chemical resistance, anti-soiling and easy to clean effect.

Application: EUROPLEX® Film HC 0F046 can be laminated as a protective top layer onto polymeric films and sheets based on PVC, ABS, PC and ASA. Decorative films protected with EUROPLEX® on top can be thermoformed and laminated on different substrates, such as PVC profiles, or used in complex shapes molding processes such as In- Molding Decoration. In labels or Graphic Arts, EUROPLEX® Film HC 0F046 can be used as a high quality clear overlay in laminate systems for high UV and weathering protection. Chemical resistant, anti-soiling and easy to clean effects are achieved.

Information Provided by Evonik CYRO. The former Evonik Methacrylates business has been sold to Röhm GmbH, although this trade name was disontinued prior to the sale.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³DIN 53479
Surface Tension 23 dynes/cm23 dynes/cmDIN 53364
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 37.0 MPa5370 psiISO 527-3
Elongation at Break >= 50 %>= 50 %ISO 527-3
Elongation at Yield 7.0 %7.0 %ISO 527-3
 
Optical PropertiesMetricEnglishComments
Haze 3.0 %3.0 %ASTM D1003
Transmission, Visible >= 92 %>= 92 %ISO 13458-2
UV Transmittance <= 1.5 %
@Wavelength 280 - 380 nm
<= 1.5 %
@Wavelength 280 - 380 nm
DIN EN 410

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIL036 / 196240

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.