MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ExxonMobil Exact™ 3132F Ethylene Alpha Olefin Copolymer
Categories: Polymer; Thermoplastic

Material Notes: Plastomers are ethylene alpha olefin copolymers that bridge the gap between elastomers and plastics. With rubber-like properties and the processability of plastic, they are used as polymer modifiers to provide unique properties in flexible packaging, molded and extruded products, and foamed compounds.  Benefits: Flexible packaging – enhanced toughness, clarity and sealing performance, Molded and extruded products – improved impact strength and flexibility, Foamed compounds – added durability to lightweight shoe mid soles  Exact™ plastomer resins for film packaging.  Exact plastomer resins for film packaging can be used in blends with polyolefins to improve the heat-sealing performance and toughness in film applications. 

Availability:  Latin America, North America. 

Additive:  antiblock: no; slip: no; thermal stabilizer: no.  Applications: blown film.  Forms: pellets.

Information provided by ExxonMobil.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ExxonMobil Method
Melt Flow 1.2 g/10 min1.2 g/10 minEstimate from data measured at other conditons.; ExxonMobil Method
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 4.00 MPa580 psiASTM D882
Film Tensile Strength at Yield, TD 3.86 MPa560 psiASTM D882
Film Elongation at Break, MD 520 %520 %ASTM D882
Film Elongation at Break, TD 650 %650 %ASTM D882
Secant Modulus, MD 0.0655 GPa9.50 ksiASTM D882
Secant Modulus, TD 0.0689 GPa10.0 ksiASTM D882
Puncture Energy 6.78 J5.00 ft-lbExxonMobil Method
Elmendorf Tear Strength MD 210 g210 gASTM D1922
Elmendorf Tear Strength TD 320 g320 gASTM D1922
Dart Drop Test 1200 g2.65 lbASTM D1709A
Film Tensile Strength at Break, MD 67.6 MPa9800 psiASTM D882
Film Tensile Strength at Break, TD 61.4 MPa8900 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 94.4 °C202 °FPeak; ExxonMobil Method
Crystallization Temperature 76.1 °C169 °FExxonMobil Method
Vicat Softening Point 83.9 °C183 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 2.1 %2.1 %ASTM D1003
Gloss 79 %79 %@ 45°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEX98951 / 238332

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.