MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
PPT BP600 NiZn Ferrite Powder
Categories: Ceramic; Oxide

Material Notes: Uses: EMI Suppressors, Wave Absorbing Tiles, Impeders, Multi-Hole Connectors, Inductors, Transformers, Converters, Choke Coils, Antennas

Electromagnetic characteristics were tested on toroid with a HP4294A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 1.50 g/cctypical
Water Absorption at Saturation 0.30 %
Particle Size 120 µmmedian granule size
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1e+9 ohm-cm
Magnetic Coercive Force, Hc 0.45 Oe
Magnetic Remanence, Br 1200 Gauss
Curie Temperature 160 °C
 
Thermal PropertiesOriginal ValueComments
Shrinkage 15.5 %
 
Processing PropertiesOriginal ValueComments
Sintering Temperature 1200 °C
@Time 7200 sec
 
Descriptive Properties
Flux Density Bs3600 GaussField Strength = 30 Oe
Initial Permeability, µi600
Q Factor (w/ 10 turns)700.1 MHz

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
PPT BP2000 NiZn Ferrite Powder
Ferrite 1, Sintered Iron-Barium Oxide Hard Magnetic Material
Iron (II, III) Oxide, Fe3O4 (Magnetite)
Ferrite 5, Sintered Iron-Strontium Oxide Hard Magnetic Material
PPT FP95 Fully Sintered Ferrite Powder

CPPT964 / 125999

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.