MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Annealed 1093°C 2 hr
Categories: Metal; Nonferrous Metal; Cobalt Alloy; Superalloy

Material Notes: Data provided by Carpenter Technology Corporation.

Annealing followed by water quench and low stress grinding prior to tensile testing.

Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting high strength, corrosion resistance, and wear resistance. BioDur CCM Plus alloy is a wrought powder metallurgy product produced by vacuum induction melting (VIM) followed by inert gas atomization and hot isostatic pressing to produce 100% dense billets. These billets are then processed by conventional steel-making practices to make finished products.

BioDur™ and CCM Plus™ are trademarks of Carpenter Technology Corporation.

Key Words: ASTM F799; ASTM F1537; ISO 5832-4; ISO 5832-12
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.28 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 334Estimated from Rockwell C for Brinell test with 3000 kg load, 10 mm ball.
Hardness, Knoop 363Estimated from Rockwell C
Hardness, Rockwell C 36
Hardness, Vickers 349Estimated from Rockwell C
Tensile Strength, Ultimate 1310 MPa
Tensile Strength, Yield 717 MPa
@Strain 0.2 %
Elongation at Break 32 %in 4D
Reduction of Area 27 %
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.8 µm/m-°C
@Temperature 0.000 - 100 °C
 13.1 µm/m-°C
@Temperature 25.0 - 300 °C
 14.7 µm/m-°C
@Temperature 25.0 - 700 °C
 16.92 µm/m-°C
@Temperature 25.0 - 1000 °C
Specific Heat Capacity 0.452 J/g-°C
@Temperature 23.0 °C
 0.590 J/g-°C
@Temperature 600 °C
 0.673 J/g-°C
@Temperature 1100 °C
Thermal Conductivity 12.766 W/m-K
@Temperature 23.0 °C
 25.264 W/m-K
@Temperature 600 °C
 35.022 W/m-K
@Temperature 1177 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.20 - 0.30 %
Chromium, Cr 26 - 30 %
Cobalt, Co 66 %as remainder
Molybdenum, Mo 5.0 - 7.0 %
Nitrogen, N 0.15 - 0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Carpenter BioDur™ CCM® Medical Implant Alloy, Annealed
Carpenter BioDur™ CCM® Medical Implant Alloy, Hot Worked
ATI Allvac® Nickelvac® TJA-1537™ UNS R31537 & UNS R31538 Nickel Superalloy, Warm Worked
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Annealed 1093°C 1 hr
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Hot Worked

NCAR34 / 15624

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.