MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Kangxi Plastics PBT-30GF PBT, 30% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled

Material Notes: Applications: Home appliance parts, lighting fixtures, internal parts of electronic products, electron component, car handle, door bolt, coil framework, relay of electric appliance, and connector injection molding products

Modified Features: Reinforced, flame retardant/reinforced

Product Features: Comply with ROHS, high mechanical strength, high rigidity, and high temperature tolerance, good performance of electric appliance, stable size, and bloom free, good appearance applicable to the precision shaping

Information provided by Wuxi Kangxi Plastics Technology Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.53 g/cc1.53 g/ccASTM D792
Linear Mold Shrinkage 0.0030 - 0.0090 cm/cm0.0030 - 0.0090 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 120120ASTM D785
Tensile Strength 130 MPa18900 psi10mm/min; ASTM D638
Elongation at Break 2.5 %2.5 %10mm/min; ASTM D638
Flexural Strength 180 MPa26100 psi2mm/min; ASTM D720
Flexural Modulus 7.50 GPa1090 ksi2mm/min; ASTM D720
Izod Impact, Notched 1.00 J/cm
@Thickness 3.20 mm
1.87 ft-lb/in
@Thickness 0.126 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
@Thickness 6.40 mm
428 °F
@Thickness 0.252 in
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
@Thickness 6.40 mm
410 °F
@Thickness 0.252 in
ASTM D648
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
 
Processing PropertiesMetricEnglishComments
Front Barrel Temperature 220 - 270 °C428 - 518 °F
Melt Temperature 235 - 255 °C455 - 491 °F
Mold Temperature 50.0 - 80.0 °C122 - 176 °F
Drying Temperature 120 - 140 °C248 - 284 °F
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hour
 
Descriptive Properties
Weather Resistant0.000624hr, ASTM D570

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKXP011 / 281787

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.