  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Dover Chemical DOVERPHOS 213 Diphenyl Phosphite
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Doverphos 213 is diphenyl phosphite (DPP). It is a liquid diaryl phosphite with a relatively low molecular weight and a high phosphorus content. Doverphos 213 can be effective in improving the color of unsaturated polyesters and as a secondary stabilizer in PVC to improve early color stability and minimize plateout during processing. Typical use levels can range from 0.1 to 1.0%.

Information provided by DoverChem

Key Words: CAS# 4712-55-4-1
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.21 - 1.23 g/cc
@Temperature 25.0 °C
1.21 - 1.23 g/cc
@Temperature 77.0 °F
Molecular Weight 234 g/mol234 g/mol
ASTM Color <= 250<= 250APHA
 
Chemical PropertiesMetricEnglishComments
Total Acid Number <= 15<= 15[mgKOH/gm]
 
Optical PropertiesMetricEnglishComments
Refractive Index <= 1.56
@Temperature 25.0 °C
<= 1.56
@Temperature 77.0 °F
 
Component Elements PropertiesMetricEnglishComments
Phosphorus, P 13.3 %13.3 %
 
Descriptive Properties
Physical FormClear liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WDOVER032 / 217651

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.