MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Desktop Metal Copper (Cu) Studio System™ 3D Printed; As-Sintered
Categories: Metal; 3D Printing/Additive Manufacturing Metal; Nonferrous Metal; Copper Alloy

Material Notes: Copper printed Processed by DMSL on Desktop Metal®’s Studio System™ is pure copper. Unlike laser-based processes such as DMLS, which often print chromium zirconium copper (CuCr1Zr), bound metal deposition (BMD) is able to print pure copper. This enables for a thermal and electrical conductivity that you would expect from pure copper. 3D printing parts in copper is the best alternative to machining which most of the time turns out to be a more expensive fabrication process because copper’s extreme ductility and cold workability lead to high tool wear and slow cutting rates. In addition, the printing with the Studio System permits new high-performance designs such as the incorporation of lattice structures or conformal cooling channels to improve heat transfer that is not possible with traditional manufacturing.

Applications:

  • Electrical Equipment
  • Automotive
  • Plumbing
  • Oil & Gas
  • Heat Transfer Applications
  • Consumer Industries

Information provided by Proto3000

Key Words: Bound Metal Deposition Binder Jetting
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.75 g/ccASTM B311
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 195 MPaASTM E8M
Tensile Stress 45.0 MPa
@Strain 0.0 %
 80.0 MPa
@Strain 3 %
 160 MPa
@Strain 12.5 %
 200 MPa
@Strain 35 %
Tensile Strength, Yield 45.0 MPaASTM E8M
Elongation at Break 37.0 %ASTM E8M
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000200 ohm-cm85.2% IACS; ASTM E1004
 
Thermal PropertiesOriginal ValueComments
CTE, linear 17.01 µm/m-°C
@Temperature 20.0 - 38.0 °C
ASTM E228
 17.15 µm/m-°C
@Temperature 20.0 - 66.0 °C
ASTM E228
 17.22 µm/m-°C
@Temperature 20.0 - 93.0 °C
ASTM E228
 17.33 µm/m-°C
@Temperature 20.0 - 121 °C
ASTM E228
 17.43 µm/m-°C
@Temperature 20.0 - 149 °C
ASTM E228
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 99.9 %
Oxygen, O 0.0100 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NPROTO894 / 322907

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.