(Viewing data as-entered.
Click here
to return)
Lubriplate 32 Turbine Oil Petroleum-Based Air Compressor Fluid
Categories:
Fluid
;
Lubricant
Material Notes:
This high-performance, zinc-free fluid meets the requirements of most centrifugal air compressors. Provides excellent oxidation resistance.
Turbine Oil 32 is available in Drums.
Information provided by Lubriplate
Key Words:
Part Number L0942-
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Viscosity Measurement
32
ISO Grade
113
Viscosity Index
Saybolt Viscosity at 100°F
152
SUS
Saybolt Viscosity at 210°F
44
SUS
Kinematic Viscosity at 40°C (104°F)
32
cSt
Kinematic Viscosity at 100°C (212°F)
5.0
cSt
Thermal Properties
Original Value
Comments
Pour Point
-10.0
°F
Flammability Test
440
[°F] Fire Point
Flash Point
390
°F
Descriptive Properties
SAE No.
10
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
WLUBR027 / 76073
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.