Description: ICOFLO 510-5008 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in masterbatch (instead of pellet), superior color development or additive dispersion can be achieved in the final concentrate. Key Characteristics: high density, medium melt flow. Information provided by ICO Polymers. A Schulman acquired ICO, Inc. in 2010. |