Hostacom CR 1171 G 2116 is a 10% mineral filled PP copolymer, with medium melt flow, high impact resistance and excellent UV resistance. Product is available as a customized color matched, pellet form. This grade is not intended for medical, pharmaceutical, food or drinking water applications. This grade is delivered in 2116 color version. Storage at high temperatures (> 50°C) and high humidity may damage the packaging.Information provided by LyondellBasell. |