Nelcote® P-650M is a polyester resin system suitable for coating on any MIL-C-9084. P-650M has good electrical and mechanical properties and has been used in a wide variety of applications, including embossing die fabrication and aircraft structural parts Key Features and Benefits: - Meets requirements of MIL-R-7575C, grades A and B
- Good electrical and structural properties
- Excellent retention of mechanical properties at elevated temperatures
Applications/Qualifications: - Embossing die fabrication
- Aircraft structural parts
- Electrical Insulation
Information provided by Park Electrochemical Corp. |