MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
SEKISUI SPI KYDEX® FST CTL Thermoplastic sheet
Categories: Polymer; Thermoplastic

Material Notes: KYDEX® FST CTL is a translucent thermoplastic sheet specifically formulated to meet all Boeing and Airbus toxicity requirements for aircraft interior components.

KYDEX® FST CTL meets all flame, smoke, and heat release requirements set forth in Federal Aviation Regulations (FAR) 25.853 paragraphs (a) and (d) as well as toxicity requirements for Airbus (ABD003) and Boeing (BSS7239). Its excellent properties make it the ideal material for two and three-dimensional aircraft components where transparent design elements are desired.

Suggested Application:

  • Monuments
  • Trim parts
  • Accent strips
  • Privacy walls
  • Counter wraps
  • Stairwell wraps
Features:
  • Increases design freedom for backlit panels and accents
  • Meets the stringent requirements of FAR 25.853 (a) and (d) in all thicknesses and colors
  • Meets toxicity smoke requirements of Airbus (ABD0031) and Boeing (BSS7239)
  • Excellent fabrication and formability characteristics
  • Allows for tight tolerance control

Information provided by SEKISUI KYDEX, LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.34 g/ccASTM D792
Water Absorption 0.150 %
@Time 86400 sec
ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 125ASTM D785
Tensile Strength 74.5 MPaASTM D638
Tensile Modulus 2392 MPaASTM D638
Flexural Strength 404.4 MPaASTM D790
Flexural Modulus 2450 MPaASTM D790
Compressive Yield Strength 87.6 MPaASTM D695
Compressive Modulus 2813 MPaASTM D695
Bearing Yield Strength <= 26.9 MPaASTM D953
 77.9 MPa
@Strain 4.00 %
ASTM D953
Poissons Ratio 0.466ASTM D638
Shear Strength 77.9 MPaASTM D732
Gardner Impact 71.2 JDrop Dart Impact, GE; ASTM D5420
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 14.8 kV/mmoil; ASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 57.8 µm/m-°CASTM E831
Deflection Temperature at 1.8 MPa (264 psi) 126 °Cannealed; ASTM D648
Smoke Density <= 200FAR 25.853(d) Part V
 
Descriptive Properties
OSU Heat Release<65/65 kW/m2FAR 25.853(d) Part V
Vertical BurnPass60 and 12 sec; FAR 25.853(a)(i) and FAR 25.853(a)(ii)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSEKIS514 / 325254

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.