MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
A. Schulman Diamond ABS/PC 8901
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: Description: Injection Molding Grade, High Impact

Information provided by Diamond Polymers, Inc.

A. Schulman has acquired Network Polymers & Diamond Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/ccASTM D792
Linear Mold Shrinkage 0.0050 - 0.0080 cm/cmASTM D955
Melt Flow 1.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
Procedure A Condition G; ASTM D1238
 4.9 g/10 min
@Load 3.80 kg,
Temperature 230 °C
Procedure A Condition I; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 111ASTM D785
Tensile Strength, Yield 6100 psichs 2 in/min; ASTM D638
Flexural Modulus 260000 psiTangent, chs 0.05 in/min; ASTM D790
Izod Impact, Notched 9.50 ft-lb/in
@Thickness 3.17 mm,
Temperature 23.0 °C
bar; ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 192 °F0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648
 217 °F0.125 in bar Annealed 4 hours at 80°C; ASTM D648
Vicat Softening Point 251 °F0.125 inch, 1 Kg; ASTM D1525
Flammability, UL94 HB
@Thickness 1.50 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 445 - 500 °F
Middle Barrel Temperature 455 - 510 °F
Front Barrel Temperature 460 - 520 °F
Nozzle Temperature 460 - 520 °F
Melt Temperature 460 - 520 °FMelt temperatures above 530°F are not recommended, and may result in color shifts and or thermal instability.
Mold Temperature 100 - 180 °FHigher mold temperature can aid flow in processing, provides a better surface finish, and creates less residual stress in the finished products.
Drying Temperature 195 - 210 °F
Dry Time 2 - 4 hour
Moisture Content <= 0.020 %
Back Pressure 50.0 - 150 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman Diamond ABS/PC 7901
A. Schulman Diamond ABS TS15v04 Injection Molding Grade, ABS/PC Alloy
A. Schulman Diamond ABS/PC 9801
A. Schulman Diamond ABSPC 7030 ABS/PC Injection Molding Grade, High Impact
A. Schulman Diamond ABS/PC FC-30

PDIAM235 / 30073

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.