MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Sharadaa Ceramics REFINSUL 13 Insulating Castables Medium/High Purity
Categories: Ceramic

Material Notes: Manufacturer produces Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistance property.

Information provided by Sharadaa Ceramics Pvt. Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 1.45 g/cc0.0524 lb/in³Dried at 110°C
Grain Size <= 6000 µm<= 6000 µm
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture  0.00588 GPa
@Temperature 1100 °C
0.853 ksi
@Temperature 2010 °F
 0.0103 GPa
@Temperature 110 °C
1.49 ksi
@Temperature 230 °F
 0.0113 GPa
@Temperature 1500 °C
1.64 ksi
@Temperature 2730 °F
Compressive Strength  2.94 MPa
@Temperature 1100 °C
427 psi
@Temperature 2010 °F
Cold Crushing
 2.94 MPa
@Temperature 800 °C
427 psi
@Temperature 1470 °F
Cold Crushing
 4.90 MPa
@Temperature 110 °C
711 psi
@Temperature 230 °F
Cold Crushing
 4.90 MPa
@Temperature 1300 °C
711 psi
@Temperature 2370 °F
Cold Crushing
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.372 W/m-K2.58 BTU-in/hr-ft²-°F
 1.34 W/m-K9.30 BTU-in/hr-ft²-°F
 1.39 W/m-K9.65 BTU-in/hr-ft²-°F
 1.51 W/m-K10.5 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Fe2O3 3.5 %3.5 %
 
Descriptive Properties
Permanent Linear Change<-0.12%1100°C
 <-0.6%1500°C
 <-0.6%800°C
 -0.7 - 0.7%1300°C
Refractoriness<1750°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CSHARA037 / 130200

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.