Key Features:- Good flow properties
- Ambient temperature curing
- Red color
- Meets UL 94V-0 flame retardant specifications
- Ideal for potting and encapsulation applications
- Excellent resistance to water and chemicals
Product Description: Master Bond Polymer System EP21FRSPLV is a two component, room temperature curable, flame resistant compound for potting, encapsulating and casting. EP21FRSPLV has a one to one mix ratio, by weight. The cured resin system features durability, toughness and high strength properties. It is remarkably resistant to thermal cycling and many chemicals including fuels, lubricants, water, acids, alkalis and salts. As per UL 94V-0 specification it is serviceable over the exceptionally wide temperature range of -51°C to 90°C. Its adhesion to metals, glass, ceramics and many plastics is excellent. The hardened compound is an electrical insulator. Color of Part A is red; color of Part B is white. EP21FRSPLV is used in applications in the computer, aerospace and related industries.Product Advantages: - Convenient mixing; one to one mix ratio; by weight
- Versatile cure schedules; ambient temperature cures
- Good flow properties; excellent for potting and Encapsulation
- Superior durability; thermal shock resistance, excellent resistance to fuels and lubricants
- Complies with UL 94V-0 flame retardant specification
- Red color for easy identification
- . Official UL temperature rating of 90°C
Information provided by Master Bond Inc. |
Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.Click here to view all available suppliers for this material. Please click here if you are a supplier and would like information on how to add your listing to this material. |