Electrical grade 105°C rated vinyl elastomer compound suitable for SEO and SJEO insulation and jacket applications per UL 62. Information provided by Georgia Gulf Georgia Gulf became Axiall Corporation, which was later acquired by Westlake Plastics. This specific grade is discontinued. |