MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

Aremco Pyro-Tape™ 682-ER High Temperature Tape Single layer polyimide film with silicone adhesive  (discontinued **)
Categories: Polymer; Adhesive; Tape

Material Notes: Applications
  • Electrical Resistance
Features
  • Electrical insulation for process instrumentation, wiring and harnesses.
  • RF induction coil insulation.
  • Transformer, terminal and connector insulation.
  • Masking gold fingers for printed circuit board wave soldering.

Vendors: Aremco’s Pyro-Tape 682-Series high temperature tapes are ideal for abrasion, chemical, electrical, and thermal insulation. Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Thickness 63.5 microns2.50 mil
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.50e+17 ohm-cm1.50e+17 ohm-cm
Dielectric Constant 3.43.4
Dielectric Strength 276 kV/mm7000 kV/in
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 260 °C500 °F
Minimum Service Temperature, Air -73.3 °C-100 °F
 
Descriptive Properties
Adhesion20 oz/in
Tape Tensile Strength30 lbs/in

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CEN® Electronic Material CV Polyimide Film, 1 Mil Thickness
CEN® Electronic Material HT Polyimide Film
CEN® Electronic Material CN Polyimide Film, 7 Mil Thickness
CEN® Electronic Material CF 120CF616 Polyimide Film
Caplinq LINQTAPE™ PIT1A

ZPAREM46 / 24310

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.