MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Polycasa XT 630 PMMA
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: QUINN XT sheets have good optical properties and a brilliant surface. QUINN XT sheets offer excellent transparency, good mechanical properties, are UV resistant, have very good weathering and ageing resistance and remain color constant for years. High impact grades, QUINN XT610, XT620, XT630, have outstanding mechanical properties and excellent impact strength. Both QUINN XT sheets and all high impact grades can be used in contact with foodstuffs, as they meet all current European food control legislation. QUINN XT sheets and the high impact grades do not contain any toxic materials or heavy metals, which may cause environmental damage or health risks. It is insoluble in water, and not subject to hazardous materials identification. QUINN XT sheets and the high impact grades are easy to recycle.

Construction Components

  • Light domes
  • Partition walls
  • Door Glazing
  • Roofing
  • Skylights for caravans

Lighting

  • Lighting control lenses
  • Domestic light fittings

Engineering Components

  • Machine housings, machine safety covers

Advertising and Signage

  • Molded letters
  • Store displays
  • Shop fittings
  • Illuminated graphics panels

Other Applications

  • Containers
  • Lettering Templates
  • Solariums
  • Sound Barrier Walls

Quinn Manufacturing Group rebranded its Plastics Division as Polycasa in 2013.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.17 g/ccISO 1183
Water Absorption 0.25 %24h/23°C - 50x50x4mm; DIN 53495 Method 1
Linear Mold Shrinkage 0.0060 - 0.0090 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 155 MPaISO 2039-1
Tensile Strength at Break 55.0 MPaISO 527-2
Elongation at Break 15 %ISO 527-2
Tensile Modulus 2.40 GPaISO 527-2
Flexural Strength 90.0 MPaISO 178
Flexural Modulus 2.40 GPaISO 178
Charpy Impact Unnotched 2.50 J/cm²ISO 179-1
Charpy Impact, Notched 0.300 J/cm²ISO 179-1
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.9
@Frequency 1e+6 Hz
Dielectric Strength 30.0 kV/mmDIN 53481
Dissipation Factor 0.030
@Frequency 1e+6 Hz
DIN 53483-2
 
Thermal PropertiesOriginal ValueComments
CTE, linear 90.0 µm/m-°C
@Temperature 20.0 °C
DIN 53752
Specific Heat Capacity 1.50 J/g-°CIEC 1006
Thermal Conductivity 0.180 W/m-KDIN 52612
Maximum Service Temperature, Air 65.0 °CContinuous Use
 85.0 °CShort Term Use
Vicat Softening Point 104 °CISO 306
Decomposition Temperature >= 280 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.492DIN 5036-3
Transmission, Visible 91 %
@Thickness 3.00 mm
DIN 5036-3
 
Descriptive Properties
Forming Temperature, Air Pressure, °C130-150
Forming Temperature, Vacuum, °C140-170

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Röhm Plexiglas® zk20 Molding Compound
Röhm Acrylite Plus® zk5BR Impact Acrylic Polymer

PSF0234 / 66585

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.