MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Wacker Semicosil® 927 F Fluoro Silicone Gel
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: SEMICOSIL® 927 F is a pourable, thermally curable, addition-curing, one-part fluoro silicone rubber that cures to a soft silicone gel.

Special features:

  • one-part, ready-to-use
  • thixotropic behavior
  • rapid heat cure
  • very low hardness (gel)
  • outstanding resistance to chemicals
Application: Embedding of electronic components in contact with oils, fuels and solvents.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.26 g/cccured; ISO 2781
 1.26 g/ccuncured; DIN 53479
Viscosity 2500 cP
@Shear Rate 10.0 1/s
ISO 3219
 6000 cP
@Shear Rate 0.500 1/s
ISO 3219
 
Mechanical PropertiesOriginal ValueComments
Penetration 50
@Load 0.00938 kg
[mm/10]; DIN ISO 2137
 
Processing PropertiesOriginal ValueComments
Cure Time 4.00 hour
@Treatment Temp. 100 °C
 30.0 min
@Treatment Temp. 150 °C
 
Descriptive Properties
Coloropaquecured
 opaqueuncured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wacker Wacker SilGel® 613 Silicone Gel
Wacker Powersil® GEL A/B Silicone Gel

PWACK9417 / 204946

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.