MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

Aremco Ceramabind™ 643-2 High Temperature Inorganic Binder
Categories: Ceramic

Material Notes: Excellent for formulating thin coatings that set at room temperature and can be raised rapidly to high temperatures

Key Words: Coatings
Vendors: Aremco’s Ceramabind materials are unique binder systems used to formulate adhesives, coatings and potting compounds for applications to 3200°F (1760°C). Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.27 g/cc1.27 g/cc
Solids Content 30 %30 %by weight
pH 11.511.5
Viscosity 30 cP30 cP
Storage Temperature 7.22 - 35.0 °C45.0 - 95.0 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 1650 °C3000 °F
 
Processing PropertiesMetricEnglishComments
Dry Time 0.5 hour0.5 hourair dry
Shelf Life 6.00 Month6.00 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aremco Ceramabind™ 875 High Temperature Inorganic Binder
Aremco Ceramabind™ 830 High Temperature Inorganic Binder
Aremco Ceramabind™ 644-S High Temperature Inorganic Binder
Aremco Ceramabind™ 644-A High Temperature Inorganic Binder
Aremco Ceramabind™ 643-1 High Temperature Inorganic Binder

CAREM81 / 622

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.