MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

HB Fuller 2532 Silicone System
Categories: Polymer; Thermoset; Silicone

Material Notes: 2532 is two-component addition type thermal conductive potting material, room temperature and heating fast cure silicone system. This material has excellent conductivity insulation, flame retardancy, weather and high temperature resistance. 2532 is formulated to function as a bonding, sealing and encapsulating material for electronic components. This material performs at temperatures ranging from -60°C to 210°C.

Features and Benefits:

  • Halogen free
  • RoHS compliant
  • Low odor and non-corrosive
  • Excellent thermal conductivity
  • Flame retardancy can meet UL94-V0
  • High adhesion to a variety of materials including, FRP, FR4, solder mask, glass, aluminum and composites
  • Excellent weather and high temperature resistance
  • Fast cure when heated

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.60 g/cc1.60 g/cc
Viscosity 3000 - 4000 cP3000 - 4000 cPPart B
 4000 - 5000 cP4000 - 5000 cPPart A
Storage Temperature 8.00 - 25.0 °C46.4 - 77.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5858GB/T531
Tensile Strength 1.80 MPa261 psi
Elongation at Break 90 %90 %GB/528
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmGB/T1692
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 210 °C410 °F
Minimum Service Temperature, Air -60.0 °C-76.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 60.0 min1.00 hourWorking time
 10.0 min
@Temperature 120 °C
0.167 hour
@Temperature 248 °F
 40.0 min
@Temperature 50.0 °C
0.667 hour
@Temperature 122 °F
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
ColorGrey
ConsistencyLow Viscosity Liquid
Mix Ratio1:1Volume
 1:1Weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHBFULL092 / 316883

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.