MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Samyang TRILOY® 210 NA PC + ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: Availability: Asia Pacific; Europe; North America

Automotive Specifications: GM QK 002411 Color: Natural; GM QK 002421 Color: Natural; IMDS ID 78784982 Color: Natural

Appearance: Natural Color

Form: Pellets

Information provided by Samyang Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³ASTM D792
Water Absorption 0.20 %
@Time 86400 sec
0.20 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inASTM D955
Melt Flow 21 g/10 min
@Load 5.00 kg,
Temperature 250 °C
21 g/10 min
@Load 11.0 lb,
Temperature 482 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 110110ASTM D785
Tensile Strength, Yield 61.3 MPa8890 psiASTM D638
Elongation at Break 220 %220 %ASTM D638
Flexural Yield Strength 79.3 MPa11500 psiASTM D790
Flexural Modulus 2.31 GPa335 ksiASTM D790
Izod Impact, Notched 6.41 J/cm
@Thickness 3.17 mm
12.0 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5.00e+16 ohm-cm5.00e+16 ohm-cmASTM D257
Dielectric Constant 3.03.0ASTM D150
Dielectric Strength 25.2 kV/mm640 kV/inASTM D149
Dissipation Factor 0.00900.0090ASTM D150
Arc Resistance >= 123 sec>= 123 secASTM D495
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Transverse to Flow 73.8 µm/m-°C41.0 µin/in-°FASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 111 °C231 °FUnannealed; ASTM D648
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSAMY11385 / 312078

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.