Supol HO125SS WK Saturn Black is a mineral-filled, scratch resistant, UV stabilized thermoplastic polyolefin (TPO) resin that is typically used for automotive interior applications. Availability: North America Application: Automotive Parts; Interior Automotive Applications Market: Automotive Processing Method: Injection Molding Attribute: Scratch Resistant; UV Stabilized Information provided by LyondellBasell. |