MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Huntsman IROGRAN® A 88 H 4622 TPU-Polyester
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Introduction: IROGRAN A 88 H 4622 is a black colored thermoplastic polyether/polyester-polyurethane for injection molding and extrusion applications. Additional characteristics of the product are high extrudability and low-adhesion surfaces.

Performance Features:

  • High hydrolysis resistance
  • Low-adhesion surfaces
  • Good melt flow
  • High production rates
  • High wear resistance
Applications: For the production of jackets for high pressure hoses, jacket material for cables hoses, profiles.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³Injection molded parts
Linear Mold Shrinkage 0.0040 cm/cm0.0040 in/inInjection molded; ASTM D955
Melt Index of Compound 75 g/10 min
@Load 21.6 kg,
Temperature 190 °C
75 g/10 min
@Load 47.6 lb,
Temperature 374 °F
MVR, [cm3/10 min]
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8888Injection molded parts; ASTM D2240
Hardness, Shore D 3636Injection molded parts; ASTM D2240
Tensile Strength at Break 39.0 MPa5660 psiInjection molded parts; DIN 53504
Elongation at Break 650 %650 %Injection molded parts; DIN 53504
100% Modulus 7.00 MPa
@Strain 100 %
1020 psi
@Strain 100 %
Injection molded parts; DIN 53504
300% Modulus 11.0 MPa
@Strain 300 %
1600 psi
@Strain 300 %
Injection molded parts; DIN 53504
Tear Strength 65.0 kN/m371 pliInjection molded parts; ASTM D624
Abrasion 4545mm3, Injection molded; ISO 4649
Compression Set  25 %
@Temperature 22.8 °C,
Time 86400 sec
25 %
@Temperature 73.0 °F,
Time 24.0 hour
Injection molded; ASTM D395
 40 %
@Temperature 70.0 °C,
Time 86400 sec
40 %
@Temperature 158 °F,
Time 24.0 hour
Injection molded; ASTM D395
 
Thermal PropertiesMetricEnglishComments
Melting Point 122 - 175 °C252 - 347 °F
 
Processing PropertiesMetricEnglishComments
Feed Temperature 25.0 - 40.0 °C77.0 - 104 °FExtrusion
Middle Barrel Temperature 165 - 190 °C329 - 374 °FExtrusion
Nozzle Temperature 170 - 200 °C338 - 392 °FExtrusion
 180 - 200 °C356 - 392 °FInjection
Adapter Temperature 175 - 195 °C347 - 383 °FExtrusion
Die Temperature 175 - 200 °C347 - 392 °FExtrusion
Melt Temperature 170 - 195 °C338 - 383 °FInjection
Mold Temperature 20.0 - 70.0 °C68.0 - 158 °FInjection
 
Descriptive Properties
Heating Zone175-195°CInjection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Huntsman IROGRAN® PS442-202 TPU-Polyester
Huntsman IROGRAN® A 92 E 4670 TPU-Polyester

PHUQ098 / 159471

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.