MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lord Adhesives PC11325 Silver Conductive Coating
Categories: Polymer; Thermoset; Epoxy; Epoxy, Electrically Conductive

Material Notes: LORD® PC11325 silver conductive coating is designed for use with tantalum capacitor electrode terminations. The composition is a silver-bearing, thermosetting epoxy body coating designed primarily for use as a conductive electrode for tantalum capacitors. It can also be used as a general-purpose conductive paint for printed circuit board repair and electromagnetic shielding applications.

Features: provides excellent rheological properties for either dip or paint applications. provides good resistance to settling; easily mixed after storage. cured film provides excellent electrical and environmental stability both initially and upon aging.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Brookfield Viscosity 500 - 600 cP
@Temperature 25.0 °C
Brookfield RVT, Spindle 2, 50 rpm
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity <= 0.000200 ohm-cm
@Treatment Temp. 150 °C,
Time 598 sec
dried
 <= 0.000200 ohm-cm
@Treatment Temp. 210 °C,
Time 1800 sec
cured
 
Processing PropertiesOriginal ValueComments
Shelf Life 3.00 Month
@Temperature 5.00 °C
from date of shipment in original, unopened container away from heat or flames
 
Descriptive Properties
AppearanceSilver Liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLORD9326 / 232682

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.