MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Pyrotek Pyrocast ALFS Abrasion-Resistant Refractory Castable
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Pyrocast ALFS refractory is a high flow, fused silica castable. At low water levels (6.5-7%), Pyrocast ALFS exhibits outstanding flow characteristics.

Applications

  • Aluminum melting equipment
  • Aluminum holding equipment
  • Transfer troughs
  • Ladle linings
  • Filter Bowls

Advantages

  • Exceptional resistance to thermal shock
  • Non-wetting to molten aluminum
  • Improved service life in molten aluminum transfer applications

Information provided by Pyrotek.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.986 g/cc
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.00950 GPa
@Temperature 954 °C
 0.0102 GPa
@Temperature >=110 °C
 0.0120 GPa
@Temperature 537 °C
Compressive Strength 34.5 MPa
@Temperature 110 °C
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 1.34 W/m-K
@Temperature 260 °C
 1.46 W/m-K
@Temperature 538 °C
 1.54 W/m-K
@Temperature 816 °C
Maximum Service Temperature, Air 1371 °C
Shrinkage 0.15 %
@Temperature 954 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Pyrotek Pyrocast AR Castable Refractory
Pyrotek Pyrocast AR-S Castable Refractory
Pyrotek Dense Fused Silica Pre-Cast Shapes
Pyrotek Pyrocast AL3 Abrasion & Alkali Resistant Refractory Castable
Pyrotek Pyrocast AR PLUS Castable Refractory

CPYRO177 / 1894

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.