MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lanthanum, La
Categories: Metal; Nonferrous Metal; Pure Element

Material Notes:

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 6.166 g/cc
 
Chemical PropertiesOriginal ValueComments
Atomic Mass 138.90551995
Atomic Number 57
X-ray Absorption Edge 0.31842 ÅK
 1.97892 ÅLI
 2.1003 ÅLII
 2.25792 ÅLIII
Electronegativity 1.1Pauling
Ionic Radius 1.016 ÅCrystal Ionic Radius for Valence +3
 1.39 ÅCrystal Ionic Radius for Valence +1
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 28
Tensile Strength, Ultimate 130 MPa
Tensile Strength, Yield 125 MPa
Elongation at Break 7.9 %
Tensile Modulus 36.6 GPa
Bulk Modulus 27.9 GPa
Poissons Ratio 0.28
Shear Modulus 14.3 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000798 ohm-cm
Magnetic Susceptibility 7.27e-7cgs/g
Critical Magnetic Field Strength, Oersted 800or alpha phase
 1096beta phase
Critical Superconducting Temperature 9.20 K~5.5-12.9 K from 0-21.0 GPa pressure; 4.88 for alpha phase. Value for ßLa is 6.00 K.
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 44.6 J/g
CTE, linear 12.1 µm/m-°C
@Temperature 20.0 °C
Specific Heat Capacity 0.1641 J/g-°CGas
 0.1951 J/g-°CCrystal
Thermal Conductivity 14.0 W/m-K
Melting Point 915 - 925 °C
Boiling Point 3464 °C
Heat of Formation 0.000 kJ/molCrystal
 431 kJ/molGas
 
Optical PropertiesOriginal ValueComments
Emissivity (0-1) 0.409
@Wavelength >=645 nm,
Temperature 867 - 918 °C
 
Component Elements PropertiesOriginal ValueComments
Lanthanum, La 100 %
 
Descriptive Properties
CAS Number7439-91-0
SolubilitySoluble in diluted Acid

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Silver, Ag
Herculoy®, High-Silicon Bronze A, UNS C65500, OSO35 Temper flat products
Herculoy®, High-Silicon Bronze A, UNS C65500, OSO50 Temper rod
Herculoy®, High-Silicon Bronze A, UNS C65500, OSO70 Temper flat products
Low-silicon bronze B, UNS C65100, H00 Temper 2 mm wire

AMELa00 / 53

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.