MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Morgan Advanced Ceramics Luminex™ 880 Mac-M0880S Technical Ceramic
Categories: Ceramic; Oxide; Magnesium Oxide

Material Notes: A porous magnesia ceramic.

Applications:

  • Domestic and industrial electrical equipment
  • Crushable bushes for electrical insulation at high temperature
  • Insulating material for thermocouples
  • Heat conductive fillers

information provided by Morgan Advanced Materials

Key Words: Technical Ceramic
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.40 g/cc0.0867 lb/in³fired
Porosity 30 %30 %open, apparent
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 15.0 MPa2180 psi3-point @ 20°C
Compressive Strength 40.0 MPa5800 psi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 1.00e+9 ohm-cm
@Temperature 600 °C
<= 1.00e+9 ohm-cm
@Temperature 1110 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 13.0 µm/m-°C
@Temperature 20.0 - 1000 °C
7.22 µin/in-°F
@Temperature 68.0 - 1830 °F
Maximum Service Temperature, Air 800 °C1470 °F
 
Descriptive Properties
Colorbuff

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CMORF8030 / 203507

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.