MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

DuPont Mobility and Materials Betaseal™ 1910-1F Adhesive
Categories: Polymer; Adhesive; Thermoset

Material Notes: Warm or cold processable, high viscosity, medium modulus, glass bonding adhesive can be used primerless on paint and glass.

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.22 - 1.26 g/cc0.0441 - 0.0455 lb/in³ISO 845
Solids Content >= 98 %>= 98 %
Viscosity 330000 - 450000 cP
@Temperature >=50.0 °C
330000 - 450000 cP
@Temperature >=122 °F
Casson; D(1s) 1.075
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 55 - 6755 - 67DIN 53505
Tensile Strength at Break 7.00 MPa1020 psiISO 1798
Elongation at Break 300 %300 %ISO 1798
Shear Modulus 0.00160 - 0.00220 GPa0.232 - 0.319 ksi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+6 ohm-cm1.00e+6 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air <= 100 °C<= 212 °FTemperature stability
Minimum Service Temperature, Air -40.0 °C-40.0 °FTemperature stability
 
Processing PropertiesMetricEnglishComments
Processing Temperature 45.0 - 60.0 °C113 - 140 °F
Shelf Life 6.00 Month
@Temperature 5.00 - 25.0 °C
6.00 Month
@Temperature 41.0 - 77.0 °F
in unopened containers. Short term storage temperatures: 0°C to +40°C.
 
Descriptive Properties
BasisPolyurethane prepolymers
ColorBlack
CompatibilityGlass
 Paint
PolymerAdhesive
Regional AvailabilityEurope
 Near East/Africa
Sagging< 30°On vertical wall
Skinning time20 - 35 Minutes.After 24 hours at 60°.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDTF9180 / 254263

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.