MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

3M Scotch-Weld™ DP600 Concrete Repair and Self-Leveling
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: 3M™ Scotch-Weld™ Concrete Repair Self-Leveling DP600 is a gray, rapid setting, two component polyurethane. It is packaged as a 1:1 ratio liquid in a duo-pack cartridge. With the squeeze of a trigger, the components are automatically mixed and easily dispensed as a bubble-free self-leveling liquid.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.02 - 1.07 g/cc0.0368 - 0.0387 lb/in³Part B
 1.14 - 1.19 g/cc0.0412 - 0.0430 lb/in³Part A
Brookfield Viscosity 1000 - 3000 cP1000 - 3000 cPPart A, CP#52 @ 100 rpm
 1100 - 6000 cP1100 - 6000 cPPart B, CP#52 @ 100 rpm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 70
@Time 3600 sec
70
@Time 1.00 hour
after cure
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °F
Minimum Service Temperature, Air -51.0 °C-59.8 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 60.0 min1.00 hourFull, 10 g. 1/4" thick @ RT
Tack-Free Time 4.00 min0.0667 hour10 g, 1/4" thick @ RT
 
Descriptive Properties
AppearanceClear YellowishPart A
 Medium-GrayCured
 Opaque BlackPart B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Applied Composites 120 Polyester SMC
ArcelorMittal Dual Phase 780 LCE Y450 Very High Strength Cold Rolled Steel
3M Scotch-Weld™ DP8005 Translucent Structural Adhesive
ArcelorMittal Dual Phase 600 Very High Strength Hot Rolled Steel
ArcelorMittal Dual Phase 600 Very High Strength Cold Rolled Steel

PMM34611 / 169358

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.