MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

Prodways TPU-70 A Powder for Laser Sintering  (discontinued **)
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Elastomeric powder with fine granulometry. Excellent elongation, high resolution, long lifecycle, good chemical resistance, high recyclability, no need for infiltration.

Hoses, grips, bellows, bumpers, seals, gaskets, tubes, toys and modeling, footwear and fashion, elastic structures.

Information provided by Prodways

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³Finished Parts
Particle Size 62 µm62 µmAverage
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7070
Tensile Strength 7.00 MPa1020 psi
Elongation at Break 21 %21 %Z direction
 350 %350 %XY direction
Tensile Modulus 0.0650 GPa9.43 ksi
Izod Impact, Unnotched (ISO) NBNB
 
Thermal PropertiesMetricEnglishComments
Melting Point 105 - 122 °C221 - 252 °F
 
Descriptive Properties
AppearanceWhite
ResistivityInsulator

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Röhm CYROLITE® Protect 2 Acrylic-polycarbonate alloy
Geon® Performance Solutions HC 2190G Polyvinyl Chloride, Flexible
Geon® Performance Solutions HC 2180G Polyvinyl Chloride, Flexible
Polyplastic Armamid® PA6 GF 30 HS-901 Nylon, 30% Glass Filled
RTP Company PermaStat® 1200-70A  Polyurethane Thermoplastic Elastomer (TPU) Anti-Static - 70 Shore A

PPRODW956 / 220974

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.