MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Evonik VESTAKEEP® D4 G PEEK, for Dental Use
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Unreinforced

Material Notes: VESTAKEEP® D4 G is natural colored, high viscosity polyether ether ketone (PEEK) that is especially designed for removable and fixed dentures, crowns and bridges.
Dry properties listed below
Industrial Sector: Medical Devices
Processing: Injection molding, Extrusion
Delivery form: Pellets, Granules
Optics: Opaque
Resistance to: Heat (thermal stability), Hydrolysis / hot water, Wear / abrasion, Fatigue resistance
Conformity: Biocompatibility, Medical application
Additives: Unfilled
Processing: Powder bed fusion
Special Characteristics: Semi-crystalline
Regulatory: US Pharmacopeia Class VI conformity
Color: Natural color
Chemical Resistance: Acid resistance, Alkali resistance, Solvent resistance, Grease resistance, Hydrolytically stable, Oil resistance, Oxidation resistance, General chemical resistance

Information provided by Evonik.

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³ISO 1183
Water Absorption 0.400 %0.400 %Sim to ISO 62
Linear Mold Shrinkage, Flow 0.00900 cm/cm0.00900 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0110 cm/cm0.0110 in/inISO 294-4, 2577
Melt Flow 12.0 g/10 min
@Load 5.00 kg,
Temperature 380 °C
12.0 g/10 min
@Load 11.0 lb,
Temperature 716 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 96.0 MPa13900 psiISO 527
Tensile Strength, Yield 96.0 MPa13900 psiISO 527
Elongation at Break 30.0 %30.0 %ISO 527
Elongation at Yield 5.00 %5.00 %ISO 527
Tensile Modulus 3.50 GPa508 ksiISO 527
Flexural Strength 110 MPa16000 psiISO 178
Flexural Modulus 3.50 GPa508 ksiISO 178
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched  0.700 J/cm²
@Temperature -30.0 °C
3.33 ft-lb/in²
@Temperature -22.0 °F
Type of failure: C; ISO 179/1eA
 0.800 J/cm²
@Temperature 23.0 °C
3.81 ft-lb/in²
@Temperature 73.4 °F
Type of failure: C; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 45.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
25.0 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1/-2
Melting Point 340 °C644 °FISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 210 °C410 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 155 °C311 °FISO 75-1/-2
Vicat Softening Point  305 °C
@Load 5.10 kg
581 °F
@Load 11.2 lb
50 K/h; ISO 306
 335 °C
@Load 1.02 kg
635 °F
@Load 2.25 lb
50 K/h; ISO 306
Glass Transition Temp, Tg 145 °C293 °F2nd heating, onset; ISO 11357
 150 °C302 °F2nd heating, midpoint; ISO 11357
 153 °C307 °FISO 11357-1/-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 370 °C698 °F
 380 °C716 °FInjection Molding; ISO 294
Mold Temperature 180 °C356 °FInjection Molding; ISO 294
 180 °C356 °F
Injection Velocity 200 mm/sec7.87 in/secInjection Molding; ISO 294
Recrystallization Temperature 285 °C545 °F10 K/min; ISO 11357
 
Descriptive Properties
Color2.6Color a, CIE
 60Color L, CIE
 8.5Color b, CIE
 Natural Color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIK7847 / 324979

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.