MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Parker Chomerics Tecknit® 73-00081 Electrically Conductive Acrylic and Polyurethane Paint
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS

Material Notes: Description: TECKNIT manufactures a highly conductive acrylic and polyurethane paints filled with silver. These coatings provide a cost effective method for shielding and grounding plastic enclosures, which are susceptible to EMI, and other applications requiring a flexible protective shield.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square <= 1.0 ohmCured
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 134 °CCured
Minimum Service Temperature, Air -54.0 °CCured
 
Processing PropertiesOriginal ValueComments
Cure Time 168 hour
@Temperature 24.0 °C
Pot Life 30 min
@Temperature 25.0 °C
Shelf Life 6.00 MonthUnopened Container
 
Descriptive Properties
ColorMetallic Gray
ConsistencyThin Paint
Coverage400 sq ftRecommended 0.002" thick
FillerAg/Glass
Final ConditionDurable Film
Number of ComponentsOne
ResinAcrylic
Volume115 in3
Weight128 oz

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHOME412 / 131122

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.