MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Dispersion Strengthened Copper Alloy, UNS C15720, H04 Temper, Flat Products
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Hard

Fabrication Properties: Excellent Suitability – Soldering, Capacity for Being Cold Worked; Good Suitability – Brazing; Fair Suitability – Butt Weld; Poor Suitability – Spot Weld, Seam Weld, Capacity for Being Hot Formed

Common Fabrication Processes: Blanking; Cold working; Drawing; Etching; Extruding; Forging; Heading; Hot isostatic pressing of powder; Hot working; Machining; Roll Threading and Knurling; Rolling; Stamping; Swaging; Upsetting

Typical uses: Amortisseur Bars in Synchronous Motors; Anodes; Cathodes; Circuit Breakers; Commutators in DC Devices; Connectors; Contact Supports; Electrical Relay Components; Grids; Heat Sinks; Helixes; Incandescent Lamp Leads; Lead Frames for Integrated Circuits; Lead wires; Microwave Tube Components; Pin Connectors; Radiators; Relay Blades; Rotor Bars; Springs, Relay and Switch; Switches; Vacuum Tube Components; Wire; X-ray Tube Components; Electrolytic Chlorine Cell Connectors; Resistance Welding Electrodes; Soldering Gun Tips

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.319 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 78.0 ksi
@Thickness 2.29 mm
 82.0 ksi
@Thickness 1.27 mm
 85.0 ksi
@Thickness 0.762 mm
 95.0 ksi
@Thickness 0.254 mm
Tensile Strength, Yield 74.0 ksi
@Thickness 2.29 mm
0.2% Offset
 78.0 ksi
@Thickness 1.27 mm
0.2% Offset
 82.0 ksi
@Thickness 0.762 mm
0.2% Offset
 92.0 ksi
@Thickness 0.254 mm
0.2% Offset
Elongation at Break 3.0 %
@Thickness 0.254 mm
 4.0 %
@Thickness 0.762 mm
 5.0 %
@Thickness 1.27 mm
 6.0 %
@Thickness 2.29 mm
Tensile Modulus 17000 ksi
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000190 ohm-cm89% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.20 µin/in-°F
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.0900 BTU/lb-°F
Thermal Conductivity 204 BTU-in/hr-ft²-°F
Melting Point 1981 °F
Annealing Point 1200 - 1800 °F
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.18 - 0.22 %
Copper, Cu >= 99.52 %
Iron, Fe <= 0.010 %
Lead, Pb <= 0.010 %
Oxygen, O 0.16 - 0.24 %
 
Descriptive Properties
Cold Work (%)640.09 in
 800.05 in
 880.03 in
 960.01 in
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC15720x3 / 292800

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.