MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Northstar Polymers MPP-A47A Liquid Castable Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Liquid

Material Notes: MPP-A47A is a room-temperature-cure liquid castable polyurethane system. This ether-base polyurethane system is used in applications such as mold-making, prototyping, production of cast parts, potting, tool-making, and many other applications. MPP-A47A is designed for an easy operation for industrial applications without special casting or heating equipment. The mixing ratio between part-A (MPN-023) and part-B (PBA-058) is 1:3 by volume. Its low viscosity also makes it easy to achieve replicating the details of the mold/original with a fine resolution. Urethane elastomer parts made of this system exhibit:
  • Fine resolution of mold details
  • Good resiliency and elongation
  • Good cut/tear resistance for its class
  • Good performance in wet environments
  • Easy-to-use room-temperature-curable
  • Small shrinkage factor

The suitable applications of MPP-A47A include stamps/patterns and concrete molds designed to transfer a decorative image to wet surfaces. Its property of small shrinkage rate provides users with a tight dimensional stability when a replication is made. It is also suitable for many other custom applications where flexibility and strength of the parts are required.

Information provided by Northstar Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 47ASTM D2240
Tensile Strength 500 psiASTM D412
Elongation at Break 520 %ASTM D412
Tear Strength 14.0 pliSplit; ASTM D624
 90.0 pliDie C; ASTM D624
 
Processing PropertiesOriginal ValueComments
Processing Temperature 70.0 - 90.0 °FPrepolymer Temperature
 70.0 - 90.0 °FCuring Agent Temperature
Mold Temperature 70.0 - 90.0 °F
Cure Time 6.00 - 8.00 hour
@Temperature 25.0 °C
De-mold Time
 24.0 - 36.0 hour
@Temperature 25.0 °C
Complete Cure Cycle
Pot Life 10.0 - 15.0 min
 
Descriptive Properties
Curing AgentPBA-058
PrepolymerMPN-023
Weight Ratio1:2.617Prepolymer to Curing Agent Ratio

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Coastal Enterprises Plus™ PBHT-15 High Density Urethane Foam
Alliance Polymers Zythane™ 3045D Thermoplastic Polyurethane Elastomer
Overview of materials for Thermoset Polyurethane, Liquid
Covestro Desmopan® 588 Thermoplastic Polyurethane
Northstar Polymers MSS-A95BQ Ester Base High Performance Polyurethane

PNORTH818 / 162534

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.