MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Evonik Polymer ST 81
Categories: Polymer

Material Notes: Applications: Polymer ST 81 addresses applications where tensile strength of >> 6N/mm² is required. This is especially important in applications that are covered by 1C and 2C-polyurethanes today. Showing an outstanding high tensile strength Polymer ST 81 allows formulators to enter markets such as wood construction, transport and automotive, assembly as well as light-weight construction.

Benefits: As Polymer ST 81 does not contain plasticizers, it offers a large variability in formulation design. It allows the formulation of both tin- and phthalate-free products. Furthermore, its excellent build-up of strength up to 10 N/mm² while being manually applicable makes it an interesting product to replace polyurethane adhesives.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 40000 cP40000 cP
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 10.0 MPa1450 psi
Elongation at Break 60 %60 %
 
Descriptive Properties
Appearancecolorless, transparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIM109 / 197313

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.