MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LyondellBasell Adflex KS 311 P Thermoplastic Polyolefin
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Adflex KS 311 P is a reactor TPO (thermoplastic polyolefin) manufactured using Lyondell Basell's proprietary Catalloy process technology. It is suitable for extrusion as well as injection molding and blow molding applications, including mechanical and decorative automotive parts requiring elastomeric type properties, like molded-in color automotive exterior components. The product is used by our customers for applications with paintable and weatherable requirements, such as injection molded fascias, claddings, bumper covers, body panels, step pads, and air deflectors. It is also used as a component in compounded materials for a wide range of industrial applications. The grade is available in natural pellet form.

Availability: Africa-Middle East; Asia-Pacific; Australia and New Zealand; North America; South & Central America

Application: Exterior Automotive Applications; Single Ply Roofing; Specialty Film; Stationery Film

Market: Automotive; Compounding; Industrial, Building & Construction

Processing Method: Cast Film; Compounding; Extrusion Blow Molding; Injection Molding

Attribute: Good Colorability; Good Flexibility; Good Moldability; Good Processability; Good Surface Finish; Low Temperature Impact Resistance

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.890 g/ccMethod A; ISO 1183-1
Melt Flow 9.50 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 46.0ISO 868
Tensile Strength at Break 15.0 MPaISO 527-1, -2
Tensile Strength, Yield 14.0 MPaISO 527-1, -2
Elongation at Break 800 %ISO 527-1, -2
Elongation at Yield 14.0 %ISO 527-1, -2
Flexural Modulus 530 MPaISO 178
Charpy Impact, Notched 1.40 kJ/m²
@Temperature -40.0 °C
Complete Break; ISO 179
 4.10 kJ/m²
@Temperature -20.0 °C
Partial Break; ISO 179
 59.0 kJ/m²
@Temperature 23.0 °C
Partial Break; ISO 179
Impact Test 14.0 J
@Temperature 23.0 °C
Multi-axial, 6.6 m/s, 3.2 mm plaque, Note: Failure Mode - Ductile; ASTM D3763
 26.0 J
@Temperature -40.0 °C
Multi-axial, 6.6 m/s, 3.2 mm plaque, Note: Failure Mode - Ductile; ASTM D3763
Tear Strength 103 kN/mASTM D624
 
Thermal PropertiesOriginal ValueComments
Melting Point 142 °CISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 53.0 °CUnannealed; ISO 75B-1, -2
Vicat Softening Point 112 °CA/50; ISO 306
 
Optical PropertiesOriginal ValueComments
Haze 82.0 %
@Thickness 1.14 mm
ASTM D1003
Gloss 76.0 %
@Thickness 1.14 mm
60°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEQS9003 / 323931

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.