MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

A. Schulman SCHULAMID® 66 MK4015H 40% Glass Fiber/Mineral Reinforced, Heat Stabilized Nylon 66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass/Mineral Filled

Material Notes:
Information provided by A. Schulman.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.47 g/cc1.47 g/ccASTM D792
Linear Mold Shrinkage 0.0050 cm/cm
@Thickness 3.175 mm
0.0050 in/in
@Thickness 0.1250 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 129.88 MPa18837 psiASTM D638
Elongation at Break 3.0 %3.0 %ASTM D638
Flexural Strength 169.84 MPa24633 psiASTM D790
Flexural Modulus 8.9915 GPa1304.1 ksiASTM D790
Izod Impact, Notched 0.534 J/cm1.00 ft-lb/inASTM D256
Izod Impact, Unnotched 4.81 J/cm9.00 ft-lb/inASTM D4812
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 254 °C489 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 225 °C437 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 290 - 310 °C554 - 590 °F
Mold Temperature 65.6 - 93.3 °C150 - 200 °F
Drying Temperature 79.4 °C175 °F
Dry Time 2 - 4 hour2 - 4 hourPredrying

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PASHU338 / 25302

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.