This product is being evaluated to ASTM E84 Class C, and ASTM D4226 impact testing for the proposed Polypropylene/ABS ASTM Siding standard (currently under review). Description/Features: - Calcium Carbonate Filled
- Medium Impact
- Medium Flow
- UV Stabilized
Processing Method: Injection Molding Information provided by PolyOne Corporation |