MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Lotte Advanced Materials TITANEX HB5502 HDPE, Blow Molding
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Extruded

Material Notes: HB5502 is a pelleted high molecular weight, high density polyethylene Hexene-1 resin for blow molding. HB5502 meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 (c) 3.1a & 3.2a.

Applications: Household and industrial chemical containers, toiletries, pharmaceutical and cosmetic containers.

Advantages: Excellent processability, excellent resistance to most chemicals and good balance between stiffness and impact strength.

Information provided by Lotte Advanced Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.953 g/ccASTM D1505
ESCR 10% Igepal® >= 60.0 hourF50; ASTM D1693
Melt Flow 1.30 g/10 minI5; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 340 MPaASTM D638
Tensile Strength, Yield 280 kg(f)/cm²ASTM D638
Elongation, Ultimate >= 700 %ASTM D638
Flexural Modulus 13000 kg(f)/cm²ASTM D790
 
Processing PropertiesOriginal ValueComments
Processing Temperature 180 °CRear zone temperature setting
 190 °CFront zone temperature setting
Die Temperature 190 °C
Head Temperature 190 °C
 
Compliance PropertiesOriginal ValueComments
FDA Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLOTT9599 / 326081

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.