MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
ALM PA 615-GF Nylon 12 SLS Prototyping Polymer, 50% Glass Filled  (discontinued **)
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, 50% Glass Fiber Filled

Material Notes:

Information provided by Advanced Laser Materials (ALM).

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Bulk Density 0.670 g/ccASTM D1895
Density 1.49 g/ccSintered Part; ASTM D792
Particle Size 50 µmAverage D50; Laser Diffraction
 30 - 100 µmRange (D10 to D90); Laser Diffraction
Melt Flow 50 g/10 min
@Load 5.00 kg,
Temperature 235 °C
3 min.; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 31.0 MPaXY direction; ASTM D638
Elongation at Break 1.6 %XY direction; ASTM D638
Tensile Modulus 4.10 GPaZ direction; ASTM D638
 4100 MPaXY direction; ASTM D638
Flexural Modulus 3100 MPaXY direction; ASTM D790
Izod Impact, Notched 96.0 J/cmASTM D256
Izod Impact, Unnotched 101 J/cmASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.0e+14 ohm-cm50% RH; 500V; ASTM D257
Surface Resistance 2.3e+14 ohm50% RH; 500V; ASTM D257
Dielectric Constant 3.7ASTM D150
 
Thermal PropertiesOriginal ValueComments
Melting Point 186 °CASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 179 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 134 °CASTM D648

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ALM PA 650 Nylon 12 SLS Prototyping Polymer
ALM PA 620-MF Mineral Fiber Filled Nylon 12 SLS Prototyping Polymer
Aluminum, Al
Overview of materials for Nylon 12
Overview of materials for Polypropylene, Molded

PALAP97h / 176029

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.