MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Versalis Clearflex® H&T CLH 150 Linear Low Density Polyethylene  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: Clearflex H&T CLH 150 is a linear low density polyethylene resin, with antioxidants, suitable for cast film extrusion.

Stretch films obtained from Clearflex H&T CLH 150 show good optical properties, high puncture and dart resistance together with optimum performances in automatic wrapping machines (pre-stretch).

Main Applications: Clearflex H&T CLH 150 is recommended to produce medium/high pre-stretch film. Moreover, the combination of high mechanical properties and low gel content, together with a low cling effect, makes Clearflex H&T CLH 150, even pure, the right choice in coextruded structures to produce high performance thin stretch film.

Information provided by Polimeri Europa.

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.919 g/cc0.919 g/ccISO 1183
Thickness 8.00 - 50.0 microns0.315 - 1.97 milRecommended
Melt Flow 2.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.5 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 10.0 MPa1450 psiISO 527-3
Film Tensile Strength at Yield, TD 10.0 MPa1450 psiISO 527-3
Film Elongation at Break, MD 400 %400 %ISO 527-3
Film Elongation at Break, TD 600 %600 %ISO 527-3
Coefficient of Friction, Dynamic >= 0.50>= 0.50ISO 8295
Elmendorf Tear Strength, MD 10.19 g/micron258.8 g/milISO 6383-2
Elmendorf Tear Strength, TD 15.285 g/micron388.24 g/milISO 6383-2
Dart Drop Test 180 g0.397 lbF50; ISO 7765-1
Film Tensile Strength at Break, MD 30.0 MPa4350 psiISO 527-3
Film Tensile Strength at Break, TD 25.0 MPa3630 psiISO 527-3
1% Secant Modulus, MD 130 MPa18900 psiISO 527-3
1% Secant Modulus, TD 140 MPa20300 psiISO 527-3
 
Thermal PropertiesMetricEnglishComments
Melting Point 120 °C248 °FInternal method
Vicat Softening Point 95.0 °C
@Load 1.00 kg
203 °F
@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= -70.0 °C<= -94.0 °FASTM D746
 
Optical PropertiesMetricEnglishComments
Haze 1.0 %1.0 %ISO 14782
Gloss 91 %91 %45°; ASTM D2457
Transmission, Visible 90 %90 %clear; thickness not quantified

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Iran Petrochemical (PCC) 09X02 Linear Low Density Polyethylene
Versalis Clearflex® H&T CLH 196 Hexene Copolymer Linear Low Density Polyethylene
Versalis Clearflex® H&T CLH 108 Octene Copolymer Linear Low Density Polyethylene
Versalis Flexirene® CL 10 U Butene Copolymer Linear Low Density Polyethylene
Versalis Flexirene® CL 10 Butene Copolymer Linear Low Density Polyethylene

PENG071 / 124465

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.