MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Udel® P-3500 LCD MB Polysulfone (PSU)  (discontinued **)
Categories: Polymer; Thermoplastic; Polysulfone (PSU)

Material Notes: Udel® polysulfone is a tough, rigid, high-strength thermoplastic with outstanding hydrolytic resistance. Udel® P-3500 LCD MB series polymers are particularly well suited for the fabrication of porous hollow fiber and flat sheet membranes using a solvent-based process. These high molecular weight polymers are used in a variety of membrane filtration applications, such as renal dialysis, water treatment, bio-processing, food and beverage processing, and industrial gas separation.

Udel® polysulfone polymers possess a number of attributes that are valued by the membrane industry, including excellent mechanical properties, stability at pH levels from 2-13, excellent resistance to caustic and good resistance to moderate concentrations of chlorine. They feature low levels of extractible and insoluble materials making them suitable for drinking water and food contact uses. They may be sterilized using steam, ethylene oxide and e-beam radiation.

Udel® P-3500 LCD MB series polymers are available in various narrow molecular weight range grades, as shown below. Each grade features reduced levels of cyclic dimer compared to the previous grade, P-3500 NT 11. This can be important in solution processing applications such as membrane production, as it leads to improved dope solution stability and reduced equipment fouling.

The Udel® P-3500 LCD MB series polymers are soluble in commercially available, water-miscible, dipolar, aprotic solvents, such as dimethylacetamide (DMAC), dimethylformamide (DMF), and N-methylpyrrolidone (NMP). These materials offer membrane producers very good control of pore size and pore size distribution, high membrane strength, and good film-forming properties.

Key Attributes: Acid Resistant; Alcohol Resistant; Alkali Resistant; Chemical Resistant; Good Toughness; High Heat Resistance; Hydrocarbon Resistant; Hydrolytically Stable

Applications: Membranes

Agency Ratings: FDA 21 CFR 177.1655; ISO 10993; JHOSPA Unspecified Rating

Injection Notes: UDEL P-3500 polysulfones may be dried before preparing solutions. Pellets can be dried in a circulating hot air oven, by spreading the pellets on trays to a 1-2 inch depth and drying for 3.5 hours at 257 to 325°F (135 to 163°C).

Information provided by Solvay Specialty Polymers.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.24 g/ccASTM D792
Water Absorption 0.30 %
@Time 86400 sec
ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 70.3 MPaASTM D638
Elongation at Break 50 - 100 %ASTM D638
Tensile Modulus 2480 MPaASTM D638
Flexural Strength 106 MPaASTM D790
Flexural Modulus 2690 MPaASTM D790
Izod Impact, Notched 69.0 J/mASTM D256
Tensile Impact Strength 420 kJ/m²ASTM D1822
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 3.00e+16 ohm-cmASTM D257
Dielectric Constant 3.02
@Frequency 1e+6 Hz
ASTM D150
 3.03
@Frequency 60 Hz
ASTM D150
 3.04
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 17.0 kV/mmASTM D149
Dissipation Factor 0.0010
@Frequency 1000 Hz
ASTM D150
 0.0060
@Frequency 1e+6 Hz
ASTM D150
 0.0070
@Frequency 60 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 56.0 µm/m-°CASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 174 °CUnannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Zone 1 302 °CExtrusion
Zone 5 316 - 338 °CExtrusion
Melt Temperature 316 - 371 °CExtrusion
Drying Temperature 135 - 163 °C
@Time 12600 sec
Extrusion
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
Availability (as of March 2019)Asia Pacific; Europe; Latin America; North America
ColorNatural Color
FormsPellets
ProcessingCast Film; Injection Molding; Solution Processing
RoHS ComplianceRoHS Compliant

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Westlake Plastics Thermalux® Film Made from UDEL® Polysulfone Resin
Westlake Plastics Radel® R Polyphenylsulfone
Syensqo (Solvay Specialty Polymers) Udel® P-3700 HC Polysulfone (PSU)
Syensqo (Solvay Specialty Polymers) Udel® P-3500 NT 11 Polysulfone (PSU)
Syensqo (Solvay Specialty Polymers) Udel® P-3500 LCD Polysulfone (PSU)

PSOL8Y5451 / 238832

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.