MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Eastman Eastar EN010 Copolyester  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Eastar copolyester EN010 is used primarily in molded thick wall European applications.

Applications/Uses

  • Packaging
  • Injection molding
  • Containers
  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Specific Gravity 1.33 g/cc1.33 g/ccASTM D792
    Linear Mold Shrinkage 0.0030 cm/cm
    @Thickness 3.20 mm
    0.0030 in/in
    @Thickness 0.126 in
    ASTM D955
     
    Mechanical PropertiesMetricEnglishComments
    Hardness, Rockwell R 112112ASTM D785
    Tensile Strength at Break 30.0 MPa4350 psiASTM D638
    Tensile Strength, Yield 55.0 MPa7980 psiASTM D638
    Elongation at Break 125 %125 %ASTM D638
    Elongation at Yield 4.0 %4.0 %ASTM D638
    Flexural Yield Strength 76.0 MPa11000 psiASTM D790
    Flexural Modulus 2.44 GPa354 ksiASTM D790
    Izod Impact, Notched  0.320 J/cm
    @Temperature -40.0 °C
    0.599 ft-lb/in
    @Temperature -40.0 °F
    ASTM D256
     0.540 J/cm
    @Temperature 23.0 °C
    1.01 ft-lb/in
    @Temperature 73.4 °F
    ASTM D256
    Izod Impact, Unnotched NBNBASTM D4812
     24.0 J/cm
    @Temperature -40.0 °C
    45.0 ft-lb/in
    @Temperature -40.0 °F
    ASTM D4812
     
    Thermal PropertiesMetricEnglishComments
    Deflection Temperature at 0.46 MPa (66 psi) 69.0 °C156 °FASTM D648
    Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C140 °FASTM D648
     
    Processing PropertiesMetricEnglishComments
    Melt Temperature 275 - 295 °C527 - 563 °F
    Mold Temperature 10.0 - 30.0 °C50.0 - 86.0 °F
    Drying Temperature 150 - 160 °C302 - 320 °F
    Dry Time 4 - 6 hour4 - 6 hour

    **
    Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

    Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    PE9033 / 35089

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.