MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

RAMPF RAKU® TOOL InnoClear™ OC-5086 Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: Water-clear, rigid polyurethane

Key Properties:

  • Excellent physical properties after RT cure
  • Free of mercury, MOCA or TDI
  • Excellent optical clarity as well as U.V. protection
  • Mixed material can be cast into either tin or platinum silicone molds
Applications:
  • For room temperature hand-batch or vacuum assisted casting methods
Cure 1: 24 hours at 77°F + 16 hours at 150°F
Cure 2: 7 days at 77°F

Information provided by © RAMPF Tooling Solutions GmbH & Co. KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³Hardener; ASTM D-792
 1.10 g/cc0.0397 lb/in³Cure 1; ASTM D-792
 1.10 g/cc0.0397 lb/in³Cure 2; ASTM D-792
 1.13 g/cc0.0408 lb/in³Resin; ASTM D-792
Viscosity 450 cP450 cPResin; ASTM D-2393
 650 cP650 cPMix; ASTM D-2393
 1300 cP1300 cPHardener; ASTM D-2393
Linear Mold Shrinkage 0.0010 - 0.0050 cm/cm0.0010 - 0.0050 in/inCure 1; ASTM D-2566
 0.0010 - 0.0050 cm/cm0.0010 - 0.0050 in/inCure 2; ASTM D-2566
Storage Temperature 15.0 - 30.0 °C59.0 - 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 75 - 8575 - 85Cure 1; ASTM D-2240
 75 - 8575 - 85Cure 2; ASTM D-2240
Tensile Strength 55.2 MPa8000 psiCure 2; ASTM D-638
 72.4 MPa10500 psiCure 1; ASTM D-638
Elongation at Break 8.0 %8.0 %Cure 1; ASTM D-638
 8.0 %8.0 %Cure 2; ASTM D-638
Tensile Modulus 1.83 GPa265 ksiCure 1; ASTM D-638
 1.86 GPa270 ksiCure 2; ASTM D-638
Flexural Strength 96.5 MPa14000 psiCure 2; ASTM D-790
 110 MPa16000 psiCure 1; ASTM D-790
Flexural Modulus 2.38 GPa345 ksiCure 1; ASTM D-790
 2.41 GPa350 ksiCure 2; ASTM D-790
Izod Impact, Notched 0.267 J/cm0.500 ft-lb/inCure 2; ASTM D-256
 0.587 J/cm1.10 ft-lb/inCure 1; ASTM D-256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 54.0 °C129 °FCure 2; ASTM D-648
 95.0 °C203 °FCure 1; ASTM D-648
 
Processing PropertiesMetricEnglishComments
Cure Time 120 - 240 min2.00 - 4.00 hourMix, Demold time
Gel Time 15.0 - 20.0 min15.0 - 20.0 minMix
 
Descriptive Properties
AspectWater ClearCure 1
 Water ClearCure 2
Mix Ratio100:57Resin: Hardener, Weight
 100:59Resin: Hardener, Volume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRAMPF126 / 317726

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.