MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Copper, UNS C43400, H06 Temper
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Good to excellent corrosion resistance. Excellent cold workability. Fabricated by blanking, drawing, bonding, forming, stamping and shearing.

Applications: electrical switch parts, blades, relay springs, contacts.

Available as flat products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.75 g/cc0.316 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 8383
Hardness, Rockwell 30T 7474
Tensile Strength, Ultimate 580 MPa84100 psi
Tensile Strength, Yield 490 MPa
@Strain 0.5 %
71100 psi
@Strain 0.5 %
Elongation at Break 5.0 %5.0 %In 50 mm
Modulus of Elasticity 110 GPa16000 ksiHard
Poissons Ratio 0.380.38calculated
Machinability 30 %30 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 40.0 GPa5800 ksi
Shear Strength 360 MPa52200 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000560 ohm-cm
@Temperature 20.0 °C
0.00000560 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.9 µm/m-°C
@Temperature 20.0 - 300 °C
10.5 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.380 J/g-°C0.0908 BTU/lb-°F
Thermal Conductivity 137 W/m-K
@Temperature 20.0 °C
951 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 990 - 1020 °C1810 - 1870 °F
Solidus 990 °C1810 °F
Liquidus 1020 °C1870 °F
Annealing Point 427 - 677 °C800 - 1250 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 425 - 675 °C797 - 1250 °F
Hot-Working Temperature 815 - 870 °C1500 - 1600 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 84 - 87 %84 - 87 %
Iron, Fe <= 0.050 %<= 0.050 %
Lead, Pb <= 0.050 %<= 0.050 %
Tin, Sn 0.40 - 1.0 %0.40 - 1.0 %
Zinc, Zn 14.3 %14.3 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Cast Iron
Titanium Grade 3
Copper, UNS C15710, 6 mm rod, 93% Cold Worked
Copper, UNS C15710

MC43400b9 / 11352

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.