MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Reynolds EZ~Spray® FlexFoam Sprayable Flexible Foam
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: Product Overview: EZ~Spray® FlexFoam is a flexible polyurethane foam compound that can be conveniently sprayed using Smooth-On’s EZ~Spray® Junior System. EZ~Spray® FlexFoam consists of two liquid components in an EZ~Spray® cartridge. When combined in a mixing ratio of one to one by volume, EZ~Spray® FlexFoam quickly cures to a solid, lightweight and durable 7 lb. (approx.) flexible foam, that can be used for a variety of special effects and industrial applications. Refer to Smooth-On’s EZ~Spray® Junior manual and video before using.

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.110 g/cc0.110 g/ccASTM D-1475
Viscosity 1000 cP1000 cPMixed; ASTM D-2393
 
Processing PropertiesMetricEnglishComments
Cure Time 10.0 min0.167 hourHandling/Tack-Free Time
 15.0 min0.250 hourDemold Time
Pot Life 0.167 min0.167 minASTM D-2471
 
Descriptive Properties
Approx. Volumetric Expansion7 times
ColorWhite
Kgs./Cubic Meter110[kg/m³]
Lbs./Cubic Foot7[lb/ft³]
Mix Ratio1A:1Bby volume
Specific Volume252[cu. in./lb.]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREYN183 / 296884

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.