MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Trinseo PULSE™ 2300 PT PC/ABS Engineering Resin
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes:

Information provided by Trinseo.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ASTM D792
Water Absorption 0.15 %
@Temperature 23.0 °C,
Time 86400 sec
0.15 %
@Temperature 73.4 °F,
Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0060 cm/cm0.0060 in/in
Melt Flow 1.0 g/10 min
@Load 3.80 kg,
Temperature 230 °C
1.0 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 48.3 MPa7010 psiASTM D638
Tensile Strength, Yield 51.7 MPa7500 psiASTM D638
Elongation at Break 80 %80 %ASTM D638
Flexural Strength 82.7 MPa12000 psiASTM D790
Flexural Modulus 2.24 GPa325 ksiASTM D790
Izod Impact, Notched  4.80 J/cm
@Temperature -29.0 °C
8.99 ft-lb/in
@Temperature -20.2 °F
ASTM D256
 6.40 J/cm
@Temperature 23.0 °C
12.0 ft-lb/in
@Temperature 73.4 °F
ASTM D256
Dart Drop, Total Energy  54.2 J
@Temperature 23.0 °C
40.0 ft-lb
@Temperature 73.4 °F
2.24 m/sec, 3 in. support, 0.5 in. dart; ASTM D3763
 59.9 J
@Temperature -29.0 °C
44.2 ft-lb
@Temperature -20.2 °F
2.24 m/sec, 3 in. support, 0.5 in. dart; ASTM D3763
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 72.0 µm/m-°C
@Temperature 29.0 - 100 °C
40.0 µin/in-°F
@Temperature 84.2 - 212 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 124 °C255 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 107 °C225 °FUnannealed; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Omni Plastics OmniCarb™ PC110 Polycarbonate
Covestro Makrolon® 2805 Polycarbonate, Injection Grade
Chi Mei Polylac® PA-757 ABS
Applied Nanostructured Solutions PC/ABS - Carbon NanoStructure Chopped Fiber Composite
MarkeTech Calcium Carbonate, Calcite (CaCO3) Optical Grade Crystal

PDWST087 / 142296

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.