MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

HT Materials KH2110 Polybutylene Terephthalate
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: Standard flow for compounding and injection molding

PBT exhibits almost instantaneous crystallization from the melt, enabling PBT and PBT based compounds, to be molded with short cycles in cooler tooling. The immediate high crystallinity also contributes to reduced post molding shrinkage, thereby enhancing dimensional stability.

Information supplied by HT Materials Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Moisture Absorption 0.200 %0.200 %
Viscosity Number 110 cm³/g1.10 dl/g
Melt Flow 16.0 g/10 min
@Load 2.16 kg,
Temperature 250 °C
16.0 g/10 min
@Load 4.76 lb,
Temperature 482 °F
Ash <= 300 %<= 300 %
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break >= 200 %>= 200 %
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 60.0 °C140 °F
 
Processing PropertiesMetricEnglishComments
Melt Temperature 437 °C819 °F
 
Descriptive Properties
Color (B)3
Color (L)> 90

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHTMAT902 / 326107

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.